DIMENSIONS |
|
|
|
|
|
|
(mm) |
Uncoated |
Coated |
Coated |
|
Nominal: |
Min: |
Max: |
|
OD(A) |
73.7 |
72.76 |
75.06 |
|
ID(B) |
38.9 |
37.46 |
39.76 |
|
Ht(C) |
12.5 |
12.14 |
13.34 |
|
|
|
|
|
|
|
|
|
|
|
Eff.Parameters |
|
Ae
mm2 |
Ie
mm |
Ve
mm3 |
|
210.00 |
165.00 |
34771 |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
INDUCTANCE |
|
|
|
|
AL value (nH/T2) |
Test conditions |
4024 ± 25% |
10kHz, 0.5 mT (For N = 5, use 0.62 mA), 25°C |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
CORE LOSSES |
|
|
|
|
PL
max |
Production lot limit
Max avg |
Test conditions |
4937 mW
(142 mW/cm3) |
4468 mW
(129 mW/cm3) |
100 kHz, 100 mT, 100°C |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
COATING |
|
|
|
|
Parylene rated for 200oC
continuous operation |
Voltage breakdown rating 2000V Min Wire to Wire |
|